Comparative investigation of similar and dissimilar AA6061/AA7075, AA6061/AA2024, and AA6061/AA5083 joints produced by continuous-drive friction welding
2238-7854
Abstract
This study considers continuous-drive friction welding to compare AA6061/AA6061, AA6061/AA7075, AA6061/AA2024, and AA6061/AA5083 joints produced under the same nominal processing conditions. Optical and scanning electron microscopy, EDS, XRD, Vickers microhardness, tensile testing, and SEM fractography were used to evaluate interface morphology, elemental redistribution, phase constitution, hardness, and mechanical response. No cracks, voids, or incomplete bonding were detected at the macrostructural and microstructural scales examined. The central interface regions contained fine, predominantly equiaxed grains, with average sizes of 6.2 ± 0.5, 4.1 ± 0.4, 3.6 ± 0.3, and 5.4 ± 0.5 μm for AA6061/AA6061, AA6061/AA7075, AA6061/AA2024, and AA6061/AA5083, respectively. EDS showed alloy-dependent redistribution of Mg, Si, Zn, and Cu; because deformation-induced mixing accompanies solid-state transport, we interpret the compositional gradients as elemental redistribution rather than diffusion alone. XRD patterns were dominated by α-Al and contained weak alloy-dependent reflections consistent with Mg 2 Si-, MgZn 2 -, and Al 2 Cu/Al 2 CuMg-related constituents; minor-phase assignments are therefore treated qualitatively. The measured interface hardness values were 84, 126, 132, and 88 HV2, respectively. Relative to the experimentally measured AA6061 base-metal hardness for each configuration, the interface hardness increased by 27.3%, 90.9%, 100.0%, and 35.4%, respectively; the AA6061/AA6061 HAZ showed only a small local decrease of about 1.5%. Tensile testing (n = 3 per configuration) gave UTS values of 280.0 ± 8.0, 485.0 ± 12.0, 405.0 ± 12.0, and 295.0 ± 9.0 MPa, respectively. AA6061/AA7075 showed the highest reported strength, whereas AA6061/AA5083 showed the highest elongation (12.0 ± 0.6%). Fracture occurred in the AA6061 HAZ for AA6061/AA6061 and AA6061/AA5083, and near the weld interface for AA6061/AA7075 and AA6061/AA2024. The results show that counterpart alloy chemistry is associated with systematic changes in interface chemistry, local hardness, and the strength-ductility balance.